Chromia Based
Saint-Gobain Coating Solutions supplies a wide range of chromium oxide-based powders with formulations tailored to meet specific process demands for optimal resistance to corrosion & wear due to abrasion, friction, fretting & erosion.

Chrome Oxide
Chrome Oxide Titania
Chrome Oxide Titania + Silica
Ruby
Nominal Chemistry | Morphology | Product No. | Nominal Size | Properties & Applications |
---|---|---|---|---|
Cr2O3 | Fused & Crushed, Rounded | #2022 | 5-15 µm | - Rounded for superior flowability - Against severe wear and corrosion - Used in printing, paper machine rolls, pump parts and chemical industry |
#2021 | 10-30 µm | |||
#2020, #2026, #2525 | 15-45 µm | |||
2023 | 15-63 µm |
Nominal Chemistry | Morphology | Product No. | Nominal Size | Properties & Applications |
---|---|---|---|---|
Cr2O3, 3% TiO2 | Fused & Crushed | #306 | 25-95 µm | - Good deposition efficiency and density - High wear and corrosion resistance - Used in pumps, shafts, seals, pistons and rolls |
#307 | 15-63 µm |
Nominal Chemistry | Morphology | Product No. | Nominal Size | Properties & Applications |
---|---|---|---|---|
Cr2O3, 4% SiO2, 3% TiO2 | Fused & Crushed | #340 | 25-95 µm | - Good deposition efficiency with easy finish - High wear and corrosion resistance, repair work - Used in pumps, shafts, seals and rolls |
#341 | 20-75 µm |
Nominal Chemistry | Morphology | Product No. | Nominal Size | Properties & Applications |
---|---|---|---|---|
Cr2O3, 25% Al2O3 | Agglomerated & Sintered | Ruby L | 20-45 µm | - Very high deposition efficiency, good flowability and less Cr6 formation - Replaces chromia in demanding applications - Used for release properties, dielectric strength and wear and impact resistance |
Ruby F | 15-40 µm | |||
Ruby VF | 10-30 µm |