Composition | NiCrBSiFeC |
Coating Hardness | Matrix 38HRC +/- 2 Carbides 370 Hv300 |
Coating Density | 8.1 g/cm3 (0.29 lb/in3) |
Coating Porosity | 3 - 5% as sprayed |
Pore Diameter | 5 to 15 µm |
Coating Roughness | 5 µm Ra |
CTE | 14.1 x 10-6/K at 700°C (1292°F) |
Melting Temperature | 1060°C (1940°F) |